Ferro Silicon alloy is used to precipitate and diffuse deoxidation in steel making.
Properties: Supply Ferro Silicon alloy is used to precipitate and diffuse deoxidation in steel making. We add a certain volume of silicon to steel to improve the strength, hardness and flexibility of steel. Ferro Silicon alloy also improves permeability of
-
-
FeSi
FeCaSi
Si
75% Min
60-65%
Al
1.5% Max
Ca
30-33%
C
0.2% Max
1% Max
S
0.02% Max
P
0.04%
-
FeSi
FeCaSi
Si
75% Min
60-65%
Al
1.5% Max
Ca
30-33%
C
0.2% Max
1% Max
S
0.02% Max
P
0.04%
-
Boron
18~23%
Al
0.5% Max
C
0.5% Max
Si
2.0% Max
P
0.05% Max
Fe
Balance
Packing
10Kg PP Woven Bag in 250Kg Seaworth Steel
-
HC FeMn
SiMn 70/15
SiMn 65/16
Mn
75% Min
70% Min
65% Min
C
7.3% Max
2% Max
2% Max
Si
1.2% Max
15% Max
16% Max
P
0.2% Max
0.2% Max
0.2% Max
S
0.02% Max
0.02% Max
0.02%
-
HC FeMn
SiMn 70/15
SiMn 65/16
Mn
75% Min
70% Min
65% Min
C
7.3% Max
2% Max
2% Max
Si
1.2% Max
15% Max
16% Max
P
0.2% Max
0.2% Max
0.2% Max
S
0.02% Max
0.02% Max
0.02%
-
HC FeMn
SiMn 70/15
SiMn 65/16
Mn
75% Min
70% Min
65% Min
C
7.3% Max
2% Max
2% Max
Si
1.2% Max
15% Max
16% Max
P
0.2% Max
0.2% Max
0.2% Max
S
0.02% Max
0.02% Max
0.02%
-
Ferrosilicon Lumps
Si:75%min/72%minAl:2.0%maxC:0.2%maxS:0.02%maxP:0.04%maxSize:10-50mm,50-100mm90%min or at buyer's option
pakage: In 1mt PP woven
-
Ferro Silicon alloy is used to precipitate and diffuse deoxidation in steel making.
Properties: Supply Ferro Silicon alloy is used to precipitate and diffuse deoxidation in steel making. We add a certain volume of silicon to steel to improve the strength, hardness and flexibility of steel. Ferro Silicon alloy also improves permeability of
-
-
FeSi
FeCaSi
Si
75% Min
60-65%
Al
1.5% Max
Ca
30-33%
C
0.2% Max
1% Max
S
0.02% Max
P
0.04%
-
FeSi
FeCaSi
Si
75% Min
60-65%
Al
1.5% Max
Ca
30-33%
C
0.2% Max
1% Max
S
0.02% Max
P
0.04%
-
Boron
18~23%
Al
0.5% Max
C
0.5% Max
Si
2.0% Max
P
0.05% Max
Fe
Balance
Packing
10Kg PP Woven Bag in 250Kg Seaworth Steel
-
HC FeMn
SiMn 70/15
SiMn 65/16
Mn
75% Min
70% Min
65% Min
C
7.3% Max
2% Max
2% Max
Si
1.2% Max
15% Max
16% Max
P
0.2% Max
0.2% Max
0.2% Max
S
0.02% Max
0.02% Max
0.02%
-
HC FeMn
SiMn 70/15
SiMn 65/16
Mn
75% Min
70% Min
65% Min
C
7.3% Max
2% Max
2% Max
Si
1.2% Max
15% Max
16% Max
P
0.2% Max
0.2% Max
0.2% Max
S
0.02% Max
0.02% Max
0.02%
-
FeSi
FeCaSi
Si
75% Min
60-65%
Al
1.5% Max
Ca
30-33%
C
0.2% Max
1% Max
S
0.02% Max
P
0.04%
-
FeSi
FeCaSi
Si
75% Min
60-65%
Al
1.5% Max
Ca
30-33%
C
0.2% Max
1% Max
S
0.02% Max
P
0.04%
-
Boron
18~23%
Al
0.5% Max
C
0.5% Max
Si
2.0% Max
P
0.05% Max
Fe
Balance
Packing
10Kg PP Woven Bag in 250Kg Seaworth Steel
-
HC FeMn
SiMn 70/15
SiMn 65/16
Mn
75% Min
70% Min
65% Min
C
7.3% Max
2% Max
2% Max
Si
1.2% Max
15% Max
16% Max
P
0.2% Max
0.2% Max
0.2% Max
S
0.02% Max
0.02% Max
0.02%